DSC1000L
DSC3000(DSC200/DSC2000) DIfferential Scanning Calorimeter is designed to determine the inner heat transition relating to temperature and heat flow, it is widely used in the field of polymer development, performance testing & quality control. DSC research and development includes the following field: glass transition temperature...
Availability date:
https://www.youtube.com/embed/gwfpFeHE3DY?si=EHCDWHL_PMXnUIwH
DSC3000(DSC200/DSC2000) DIfferential Scanning Calorimeter is designed to determine the inner heat transition relating to temperature and heat flow, it is widely used in the field of polymer development, performance testing & quality control. DSC research and development includes the following field: glass transition temperature, melting point, cold crystallization, crystallization, phase transition, oxidation induction time (OIT).
Main features:
1. New designed oven structure ensures high resolution and good stability of base line;
2. Air flow meter may control the air flow rate accurately; the test data can be recorded into the database directly;
3. The instrument is bilateral control, may be controlled by both main frame and software. User-friendly interface, easy operation.
Technical parameters:
1. DSC range: 0 ~ ±500mW
2. Temperature range: -100°C~800°C Liquid nitrogen refrigeration
3. Heating rate: 1 ~ 80 °C / min
4. Temperature resolution: 0.1 °C
5. Temperature fluctuations: ±0.1°C
6. Temperature repeatability: ±0.1°C
7. DSC noise: 0.01μW
8. DSC resolution: 0.01μW
9. DSC accuracy: 0.1 u W
10. DSC sensitivity: 0.1 u W
11. Control Mode: Rising temperature, constant temperature, cooling temperature (full automatic programmed control)
12. Curve scanning: Rising scan, *cooling scan
13. Atmosphere control: Embedded digital flow meter & Software control
14. Display:24 bit color 7 inches LCD touch screen display
15. Data interface: standard USB connector
16. Parameter standard: equipped with standard material, with a key calilbration function, the user may correct temperature and heat enthalpy
17. The warranty: Five years
18. Note: * for selecting projects, all technical indicators can be adjusted according to customers' demand