DSC3000C/DSC3000U
Availability date:
Product Description
DSC is a differential indicator with the highest precision introduced by the company. The sensor adopts imported E couple with high sensitivity. The signal acquisition circuit is shielded and protected, with strong anti-interference and high baseline stability. The differential scanning calorimeter is a touch screen type, which can perform glass transition temperature test, phase transition test, melting and enthalpy test, product stability, oxidation induction period test. Wide range of applications
Technical features
Technical Parameters
MODEL | DSC3000C | DSC3000U |
Temperature range | -40°C~ 600°C | -70°C~ 600°C |
Temperature resolution | 0.01°C | 0.01°C |
Temperature fluctuation | ±0.01°C | ±0.01°C |
Temperature repeatability | ±0.1°C | ±0.1°C |
Heating rate | 0.1~100°C/min | 0.1~100°C/min |
Cooling rate | 0.1~20°C/min | 0.1~40°C/min |
Constant temperature time | program setting ≤24h | program setting ≤24h |
Temperature control method | heating scan, constant temperature multi-stage, cooling scan (automatic program control) | heating scan, constant temperature multi-stage, cooling scan (automatic program control) |
DSC range | 0~±800mW | 0~±800mW |
DSC resolution | 0.01uW | 0.01uW |
DSC accuracy | 0.001mW | 0.001mW |
Power supply | AC220V/50Hz or customized | AC220V/50Hz or customized |
Atmosphere control gas | nitrogen, oxygen (automatically switches) | nitrogen, oxygen (automatically switches) |
Gas flow | 0-300mL/min | 0-300mL/min |
Gas pressure | 0.3MPa | 0.3MPa |
Display mode | 24bit color, 7-inch LCD touch screen display | |
Data interface | standard USB interface | |
Parameter standard | equipped with standard materials (indium, tin, lead), users can calibrate the temperature | |
Note | The instrument has multiple sets of thermocouples, one set of test sample temperature, and one set of test instrument internal ambient temperature. |
Part of the sample test pattern